Before the Pengawetan |
Penampilan | whiteTampal |
tack-free time(Min) | ≤10 | |
extrudability(g/s,25°C) | 5~11 | |
Menyembuhkan sepenuhnya masa(d) | 3~7 | |
After the Pengawetan |
Relative density(g/cm3) | 1.40~1.45 |
Tkekuatan ensile (MPa) | ≥2.5 | |
Break elongation(%) | ≥500 | |
Shear strength(MPa) | ≥2.0 | |
Kekerasan(Pantai A) | 45~55 | |
The general use of temperature range(°C) | -60~200 | |
Volume resistivity(Ω·㎝) | ≥1×1014 | |
Dielectric strength (kV/·mm) | ≥14 |